Properties
key.properties.Title |
|
|---|---|
| Density | 0.960 g/cm3 |
| Melt Index (g/10min @190°C/2.16 kg (ASTM D1238)) | 27 |
app.properties.Title |
|
|---|---|
| Anti-block | No |
| Slip | No |
typical.properties.Title |
|
|---|---|
| Brittleness Temperature in °C(°F) | -60 (-76) |
| Density Range | .951-.960 |
| ESCR-Environmental Stress Crack Resistance (10% IGEPAL) | 220 hr |
| ESCR-Environmental Stress Crack Resistance (100% IGEPAL) | > 1100 |
| Fabrication Method | Blow Molding |
| Melting Point, DSC (Dow Method) in °C(°F) | 133 (271) |
| Vicat Softening Point in °C(°F) | 131 (268) |